p-type bismuth telluride, thermoelectric material pellet
product description
1. MATERIAL OVERVIEW
Characteristics:
Bismuth telluride is a compound of tellurium and bismuth. When alloyed with selenium or antimony, it acts as an efficient thermoelectric material suitable for portable power generation or refrigeration. It is a narrow gap layered semiconductor with a trigonal unit cell. It mainly occurs in a rare mineral tellurobismuthite. It is produced by sealing bismuth and tellurium metals in a quartz tube under vacuum.
Applications:
Bismuth telluride finds applications in the following:
Power generation or cooling applications
Topological insulators.
Pellet Regular size: 1.6*1.6*2.0mm,1.4*1.4*1.7mm,5*5*5*5mm,10*10*10mm and so on
Also could produce small size much less than 1.00 mm like 0.35mm and so on
bar/ingot diameter is 28-35mm
We could also produce according to customer requirement
Welcome to contact us
2. GENERAL PROPERTIES
Symbol:
Bi2Te3
CAS:
1304-82-1
Atomic Weight:
800.76
Group
Bismuth – 15
Tellurium - 16
Crystal Structure
Hexagonal-Rhombohedral
Lattice Constant
a = 4.38 Å
c = 30.45 Å
Density:
7.73 g/cm3
Melting Point:
585°C
Mohs Hardness
1.8
Electron Mobility
1140 cm2/Vs
Hole Mobility
680 cm2/Vs
Thermal Conductivity
3 W/mK
3. Specification
P-type ingot:
1. Purity: 99.99%
2. Thermal conductivity (k): 1.2-1.6w/m.K
3. Seebeck (S) : 200-230 uV
4. Electrical conductivity (rou): 850-1250
5. Figure of merit (Z): 2.55- 3.4x10-3.K-1.
6. ZT>=1.1@300K
N-type ingot:
1. Purity: 99.99%
2. Thermal conductivity (k): 1.2-1.6w/m.K
3. Seebeck (S) : 205-235 uV
4. Electrical conductivity (rou): 850-1250
5. Figure of merit (Z): 2.34-3.2x10-3. K-1.
6. ZT>=1.1@300K