PEO/Plasma Electrolytic Oxidation
Specification: Product NamePPOLY ETHYLENEOXIDE(PEO)AppearanceWhite powderMolecular weight4-6million
Solventcontentless than 1%Granularity ( ≥ 20mesh)96.00%MinApparent density (kg/L) :0.300MinFlowtime (S/30g)Max6.00
Application: Used as the Disperser Agent and Retention Agent in Papermacking Industry and oil drilling field.
PEO Using Method:
Disperse PEO in water, during the dissolving of 2 ~ 3 hours, after ripening, then do dilution for 10 ~ 30 times in the dilution tank, and then put the solution into the pulp flowing box or other suitable location. In order to achieve better results, it is recommended that the joining point near the pulp flowing box as much as possible.