Product Description
Product parameter
Wire mesh Ripple 500X Figure 1-1figure1-2And get the following form:The results show: Foamed SiC mass transfer tray does not exist weeping phenomenon, wet and dry plate pressure drop lower than the F1 floating valve tray, the clear liquid height of it higher than the F1 floating valve tray. In addition, the entrainment of foamed SiC mass transfer tray is also smaller than the F1 floating valve tray. These results show that the SiC mass transfer tray is a new type of high efficiency tray.
Other Product
Product Uses
about Us
Certifications
Production Packing