1.Material:
Our tyre reclaim rubber is made fromthe wastetyre scrap absolutely.
2.Tensilestrength:
Strengthofblackreclaimedrubberisfrom4Mpato16Mpa ,180% -480% elongation.
3.Type:
Eachgradehavetwosmell type : Smell grade & Odorless grade ,
Superfinereclaimedrubber (60 mesh): 4Mpa - 16Mpa.
Tensilestrength
Elongationpercentage
Mooneyviscosity
Ashcontent
≥MPA
≥%
ML100°C@1+4
≤%
4.0MPA
220%
50-65
16
5.0MPA
250%
50-65
15
6.0MPA
260%
50-65
15
7.0MPA
280%
50-65
15
8.0MPA
290%
50-70
13
9.0MPA
310%
50-70
12
10.0MPA
350%
50-70
11
11.0MPA
370%
50-70
10
12.0MPA
390%
50-70
9
14.0MPA
450%
50-70
8
16.0MPA
470%
50-70
7.5