Business Type:
Manufacturer/Factory,Trading Company,Distributor/Wholesaler
Business Range:
Fresh Fruits, Dairy Products, Grains and Nuts, Scraps, Oil
Establishment:
2016
R&D Capacity:
OEM, ODM, Others
Terms of Payment:
LC, T/T, D/P, Paypal, Western Union
Main Markets:
South Asia, Mid East, Eastern Europe
OEM/ODM Service
Sample Available

We strives towards optimally satisfying the needs of our clients by means of multidisciplinary expertise, professional service provision and the application of best practices. Our Products are fully I...

1
    YRS
General Supplier
Supplier Homepage Metallurgy, Chemicals, Rubber & Plastics Minerals & Metallurgy Lead Lead concentrate ,lead concentrate price,lead silver concentrate

Lead concentrate ,lead concentrate price,lead silver concentrate

Get Latest Price
Min. Order / Reference FOB Price
100 MetricTon US $500.00/ MetricTon
Local Area: South Africa
R&D Capacity: OEM, ODM, Other
Payment Terms: LC, T/T, D/P, Paypal, Western Union
Brand: Lead concentrate
Model Number: concentrate
Type: Lead Bar
Weight: 11.34g/cm3

Lead concentrate ,lead concentrate price,lead silver concentrate
Lead concentrate ,lead concentrate price,lead silver concentrate
Pb min.55% , Typical 60%
Ag min.600 grams , Typical 1000 grams
Our underground mine produce approximately 150 tons of ore per month. The primary mining methods are cut and fill and longhole stoping. At Izmir, the ore is processed on site at a mill, which produces lead, zinc, and bulk concentrates.
Sample Code
Zn%
Pb%
Sn%
Fe%
L.O.I%
70
Not Detected
52.91
4.88
3.22
Not Detected

Pb min.55% , Typical 60%
Ag min.600 grams , Typical 1000 grams
Lead-Zinc ore : (Pb+Zn) 30%up and Ag 0.05%up
Lead concentrate : Pb 55%up and Ag 0.15%up
Zinc concentrate 50%up
Lead Concentrate
Ore is recovered by blasting then dumping, followed by crushing and finally hoisting to the surface for treatment. In mining, the ore is extracted by drilling or blasting and then crushed and ground. The ore is then treated using extractive metallurgy. The Froth flotation process separates the Lead and other minerals from the waste rock (tailings) to form a concentrate. The concentrate, which can range from 50% to 60% Lead, is dried and then treated using pyrometallurgy. The concentrate is sintered before being smelted in to produce a 97% Lead concentrate. The Lead is then cooled in stages which causes the lighter impurites (dross) to rise to the surface where they can be removed. The molten Lead bullion is then refined by additional smelting with air being passed over the Lead to form a slag layer containing any remaining impurities and producing 99.9% pure Lead.

Send your message to this supplier

*From:
To:
TIFFANY ANDERSON GROUP PTY LTD
*Message:

Enter between 10 to 1,000 characters.

*Email code:
This is not what you are looking for? Post a Sourcing Request Now